In above equation, F is the applied force (kgf), D is diameter of indenter (mm) and d is diameter of indentation (mm).

Figure 7 showed the hardness results for the specimens with different welding currents. From the result, the hardness of the HAZ did not grow until it reached the base material. The highest value of BHN for base metal was 187 that by specimens with welding current 90, 100 and 110 A with angle of bevel was 45° and no bevel. The highest value of BHN for HAZ area was 170 A shown by specimens with welding parameters 100 A at no bevel, 110 A at 45° bevel angle and 120 A both with no angle and 45° bevel angle. The result data showed that 120 A was the highest value of BHN on the HAZ area. High BHN values show that the indention diameter is small. This means that, the strength of the specimen or material surface is great.

Fig. 7Hardness Brinell number versus welding current



Download



Copyright Disclaimer:
This site does not store any files on its server. We only index and link to content provided by other sites. Please contact the content providers to delete copyright contents if any and email us, we'll remove relevant links or contents immediately.